What is biofouling
The settlement and build-up of organisms on wet structures in marine environments is known as biofouling. Barnacles and other marine organisms that adhere to ship hulls and marine structures are commonly known forms of biofouling. Power plants and water treatment facilities that use water from rivers and the sea can be impacted by biofouling as well.
Biofouling organisms can be categorized into two groups: macrofouling, which covers plants and animals such as barnacles, mollusks, tubeworms, and green weed; and microfouling, which is comprised of unicellular algae and bacteria also known as slime. In addition to causing hydrodynamic drag for ships and industrial processes that rely on optimum water flow, biofouling also reduces the accessibility of steel and concrete surfaces for corrosion inspections, which affects marine structures such as ships; floating production, storage, and offloading (FPSO) vessels; offshore wind tower foundations; and offshore oil and gas structures. Biofouling is known to cause various industrial problems, such as corrosion, increased drag force, and reduced heat transfer efficiency. Once biofouling has occurred, removing it can be very difficult, and risks include damaging the underlying protective coating.
Coating technology to deter biofouling
A biocide-free, advanced fluoropolymer fouling-release coating technology has been developed by AkzoNobel Marine & Protective Coatings to deter the formation of both macro- and microfouling on marine structures and industrial processes. According to the company, easy removal of biofouling is important for corrosion control. On static structures, such as the steel legs of an offshore oil platform or the hull of an FPSO, the structural integrity of the welds need to be visually inspected and assessed. If the substrate is covered in biofouling that isn’t easily removed, a large amount of force is required to scrape it off, which may damage the underlying protective coating and leave the substrate vulnerable to corrosion.
Biofouling traditionally has been controlled with antifouling coatings. These include coatings that release active biocides into the water to deter the settlement of organisms; and biocide-free, “self-cleaning” fouling-release coatings that influence the adhesion strength of fouling organisms so they fall off the coating or are swept off the coating by water flow. AkzoNobel explains that silicone-based coatings were the first commercially available biocide-free fouling-release coatings. They feature a smooth, hydrophobic (water repellant) surface and are very effective for controlling macrofouling; however, they are less successful in preventing microfouling build-up and are susceptible to moderately heavy microfouling, which is particularly detrimental for industrial processes.
AkzoNobel notes that while these fouling release technologies have not been 100% fouling free, they do have good resistance to growth of weed and barnacle types of fouling, but slime fouling is has not been fully deterred, and any type of fouling will have an impact on the hydrodynamic efficiency of a surface.
Silicone hydrogel coatings with surfaces that are highly hydrophilic (show a strong affinity for water) have been evaluated as fouling-release coatings and proved to be successful at inhibiting microfouling over a short time period. Their high affinity for water, however, limits the service life of these coatings because of film dissolution in the surrounding environment.
These issues were addressed by the development of a fluoropolymer fouling-release coating technology that creates an amphiphilic surface, which is a combination of hydrophilic and hydrophobic surfaces. Marine organisms prefer either a hydrophobic or a hydrophilic surface, depending on the organism, so a completely hydrophobic or hydrophilic surface will cause preferential settlement of fouling organisms, explains the company.
The amphiphilic nature of the fluoropolymer technology creates an inhospitable surface that disrupts settlement and influences the adhesion of a wide range of fouling organisms. The amphiphilic properties also contribute to a longer service lifetime of the fouling-release coating. The fluoropolymer fouling-release coating demonstrated better antifouling performance for macrofouling than traditional antifouling technologies; and while it showed better microfouling inhibition than silicone-based technologies, the researchers at AkzoNobel felt its performance for slime control could still be improved.
Study of biofilm helped solve for slime build-up
The settlement and release of macrofouling is influenced by several coating properties and it is well documented that a coating’s surface chemistry and surface charge, thickness and modulus, roughness, and color all affect its effectiveness. The specific parameters that affect the settlement and adhesion of microfouling on a coating, however, were not as well understood. As a result, an extensive study was undertaken that examined the composition and diversity of biofilms found on marine structures and evaluated the specific coating properties that influence slime adhesion. Knowledge attained from this study was used to design and synthesize a customized, high-performance fluoropolymer that was incorporated into the advanced fluoropolymer fouling-release coating. “The technology we’re talking about here is the first one that can really deter the build-up of slime,” adds AkzoNobel.
With a better understanding of the characteristics that influence slime adherence, the coating formulators were able to optimize the amphiphilic nature of the advanced fluoropolymer technology—the size and distribution of different surface energy regions were more pronounced, which improved the coating’s slime release properties. “While the surface is amphiphilic, it has more of a hydrophilic characteristic, and that is what deters the slime adhesion,” says the company’s fouling control team leader. Although the amphiphilic characteristic is not unique for a coating, it is the way hydrophobic and hydrophilic properties are balanced in this advanced fluoropolymer coating that is unique. “We have really pushed the boundries with this technology.”
New lab tests played role in fluoropolymer coating’s development
While the advanced fluoropolymer coating technology was being developed, researchers with AkzoNobel designed several new laboratory test methods to accurately measure the coating’s slime deterrence and release performance under hydrodynamic water flow in a range of simulated operating conditions.
• To grow slime on test panels, a multispecies slime culturing reactor was developed.
• Several field tests were carried out to determine the adhesion strength as well as the percentage of macrofouling settlement.
See detailed lab test results and their impact on the development of the coating.
To achieve the smooth surface that performs best for fouling release, the advanced fluoropolymer coating is normally applied by an airless sprayer at a thickness of 150 µm over two 150-µm thick coats of an anticorrosion epoxy coating that is topped with a 100-µm thick tie coating, and cured under atmospheric conditions.
For more information on corrosion in the maritime industry sign up for a free subscription to NACE’s Maritime News, a triannual, digital publication providing information related to the causes of maritime corrosion and coating solutions for its mitigation.
Source: Originally appeared on materialsperformance.com as “Advanced Fluoropolymer Fouling-Release Coating;” adapted from CORROSION 2014 paper no. 4468, " Novel Slime Release Biocide Free Technology,” by L. Tyson and I. Fletcher, AkzoNobel Marine & Protective Coatings.
FREE DOWNLOADS
White Paper: An Action Plan for Reducing Pipeline Failures, Costs with Corrosion in the Water Sector
Special Report: The Future of Corrosion Control, Insights from the Experts
Get Updates
Featured Articles
Categories
- 2024 Olympics (1)
- 2024 Water Resource Development Act (1)
- Abrasive Blasting (1)
- Advanced coating materials (9)
- Advanced Corrosion Control in Oil and Gas Industry (2)
- Advocacy (2)
- AI (2)
- Aircraft (1)
- Alkanization (1)
- AMPP (4)
- AMPP Annual Conference + Expo (2)
- Ampp Chapters (1)
- AMPP conference (1)
- AMPP logo (1)
- Ampp Membership (1)
- Ampp Standards (1)
- Amusement parks (4)
- Architectural (1)
- Architectural Coatings (2)
- Artificial Intelligence (1)
- Asset integrity (10)
- Asset maintenance (3)
- Asset Protection (1)
- Bim Software (1)
- Biodeterioration of materials (5)
- Biofouling (4)
- Blasting (1)
- Bridges (3)
- career development (1)
- cathodic protection (1)
- Cathodic Protection-CP (16)
- Ceramic epoxies (1)
- Certification (3)
- Chemical Injection (1)
- Civil Engineering (1)
- Coating inspector (1)
- Coating inspector jobs (1)
- Coating inspector program (1)
- Coatings (13)
- Coatings Application (2)
- Coatings failures (2)
- Coatings Industry (2)
- Coatings inspector (2)
- Coatings measurement and inspection (9)
- Coatings Systems (1)
- Cold stress (1)
- Concrete (12)
- Conference and Events (2)
- Corrosion (16)
- Corrosion Basics (5)
- Corrosion Control (15)
- Corrosion Control and Management (23)
- corrosion engineering (1)
- Corrosion Essentials (19)
- corrosion mitigation (1)
- Corrosion Prevention (6)
- Corrosion Under Insulation (1)
- cost of corrosion (1)
- Crevice Corrosion (1)
- Cui (1)
- Data Monitoring (1)
- Department of Defense (3)
- Deposition corrosion (1)
- Dissimilar Metal Corrosion (1)
- Dissolved gases (1)
- DoD (3)
- Education (2)
- Energy industry (9)
- entertainment industry (1)
- Epoxy (2)
- Fireproofing (1)
- Flexible coatings (2)
- Flint, Michigan (1)
- Fluoropolymer coating (3)
- Forms of Corrosion (4)
- Freshwater salinization (1)
- Galvanic (1)
- Galvanic Corrosion (3)
- General Corrosion (2)
- Hand tools (1)
- Industrial Application (3)
- Industrial Safety (2)
- Industry Best Practices (1)
- Industry Standards (1)
- infrastructure (2)
- Inspection (1)
- integrity management (1)
- Intergranular Corrosion (1)
- Intumescent Coatings (1)
- key note speaker (1)
- Machine Learning (1)
- Maintenance (2)
- Maritime Coatings (11)
- Maritime industry (11)
- Master Painters Institute (2)
- materials performance (1)
- Membership (2)
- Membership Benefits (2)
- Michio Kaku (1)
- Microbiological forms (1)
- Microbiologically influenced corrosion-MIC (11)
- Military (2)
- Mineral constituents (1)
- MPI (2)
- mpi training (1)
- Navy (1)
- Non-Destructive Testing (1)
- Oil and Gas (2)
- Oil Fields (1)
- Organic matter (1)
- Oxgen (1)
- Paint and Protective coatings (32)
- Paint specification (1)
- Personal Protective Equipment (3)
- Petrochemical Plant Fireproofing Methods (1)
- Petrochemical Plants (1)
- Pipeline (2)
- Pitting Corrosion (2)
- Pitting Detection (1)
- Power plant (1)
- Power tools (1)
- PPE (3)
- professional development (1)
- Protective Coatings (5)
- quality assurance (1)
- Real-Time Corrosion Monitoring in Oil Fields (1)
- Rebar Corrosion (1)
- rectifier (1)
- Reliability (1)
- Remote monitoring and drones (4)
- Repaint (1)
- Restoration (1)
- ride maintenance (1)
- Road deicers (1)
- Roads and bridges (1)
- Roller coaster (1)
- Rust (1)
- sacrificial anodes (1)
- Safety (5)
- Safety Standards (2)
- Salt pollution (1)
- Sensors (1)
- Ship Coatings (9)
- Shiptanks (1)
- Standards (9)
- Standards Committees (1)
- Steel (7)
- Steel Reinforcement (1)
- Stress Corrosion Cracking (1)
- Structural Steel (1)
- Surface Preparation (13)
- Sustainability (1)
- Sustainability and corrosion (7)
- Tools (1)
- Turbine (1)
- Types of Corrosion (1)
- Uniform Corrosion (1)
- us army core of engineers (1)
- Water crisis (1)
- Water pipe corrosion (1)
- Water quality (1)
- Water tank coatings (5)
- Water/treatment infrastructure (20)
- Waterway salinity (1)
- Workforce development (1)
- WRDA (1)